Reference Cu P Ag Melting Range °C Operating Temp °C Density g/cm3 Tensile Strengh N/mm² AWS5.8 EN1044 DIN8513 BS1845 NFA 81-363 EN17672
AKA 0.4 0.4 93.6 6 710-740 710 8.1 250 - - - - - -
AKA 1 1 92.5 6.5 645-810 710 8.1 250 - - - 07B2 - -
AKA 1 G 1 92.5 6.5 645-810 710 8.1 250 - - - 07B2 - -
AKA 2 2 91.7 6.3 645-825 740 8.1 250 BCuP-6 CP 105 L-Ag2P 06B1 CP2 CuP 279
AKA 2 G 2 91.7 6.3 645-825 740 8.1 250 BCuP-6 CP 105 L-Ag2P 06B1 CP2 CuP 279
AKA 5 5 89 6 645-815 710 8.2 250 BCuP-3 CP 104 L-Ag5P 06B2 CP4 CuP 281
AKA 5 G 5 89 6 645-815 710 8.2 250 BCuP-3 CP 104 L-Ag5P 06B2 CP4 CuP 281
AKA 15 15 80 5 645-800 700 8.4 250 BCuP-5 CP 102 L-Ag15P 05B1 CP1 CuP 284
AKA 15 G 15 80 5 645-800 700 8.4 250 BCuP-5 CP 102 L-Ag15P 05B1 CP1 CuP 284
AKA 18 18 74.95 7.05 645-650 650 8.6 250 - CP 101 - 07B4 - CuP 286
G = NON Sparkling Alloy for better fluidity and capillarity to improve wetting area and reduce leak risks.

AKA produces diferent types of Copper Phosphorus Alloys With Silver. Some of them could be missing in this table, if you do not find the alloy you are looking for, do not hesitate to consult us : info@akaonline.eu